Extraction of iron, copper, zinc and aluminium JEE Main PYQ
21 Extraction of iron, copper, zinc and aluminium JEE Main PYQ from 2012 to 2023, newest first. Single correct option: 20. Numerical answer: 1. Try each one first, then open the answer and solution under it.
Not in the JEE Main syllabus. Isolation of Metals (Metallurgy) was removed from the JEE Main chemistry syllabus from the 2024 exam and is not in the 2027 syllabus. The questions here were asked up to 2023. The chapter is still in the JEE Advanced syllabus. Deleted chemistry chapters, one by one.
Extraction of iron, copper, zinc and aluminium questions, newest first
JEE Main 202311 Apr Shift 1
Single correct optionMarks +4, -1
In the extraction process of copper, the product obtained after carrying out the reactions (i) 2Cu2S+3O22Cu2O+2SO2 (ii) 2Cu2O+Cu2S6Cu+SO2 is called
ABlister copper
BReduced copper
CCopper scrap
DCopper matte
Show answer and solution
Answer: (A)
These two reactions take place in the Bessemer converter, where copper matte is blown with air: part of Cu2S is oxidised to Cu2O, which then reacts with the rest of Cu2S (self reduction) to give copper metal. As the copper solidifies, the dissolved SO2 escapes and leaves blisters on the surface, so the product (about 98 to 99.5 percent Cu) is called blister copper. Matte is the starting material, not the product. The answer is (A).
In Hall-Heroult process, the following is used for reducing Al2O3 :-
AMagnesium
BNa3AlF6
CGraphite
DCaF2
Show answer and solution
Answer: (C)
In the Hall-Heroult process alumina dissolved in molten cryolite is electrolysed with graphite electrodes. Al deposits at the cathode, and the oxygen set free at the graphite anode burns the carbon to CO and CO2, so the overall change is 2Al2O3+3C4Al+3CO2. The carbon of the graphite is therefore consumed as the reducing agent; cryolite and CaF2 only lower the melting point and raise conductivity. So the answer is graphite, option (C).
Among following compounds, the number of those present in copper matte is A. CuCO3 B. Cu2S C. Cu2O D. FeO
Numerical answer. Work it out before you open the answer.
Show answer and solution
Answer: 1 (exact integer)
Copper matte is the product of smelting the roasted sulphide ore with silica in the reverberatory furnace. It is a fused mixture of Cu2S with a small amount of FeS. Any Cu2O formed is converted back to Cu2S by FeS, FeO goes into the slag as FeSiO3, and the carbonate does not survive the heating. Of the four, only Cu2S is present, so the answer is 1.
In the extraction of copper, its sulphide ore is heated in a reverberatory furnace after mixing with silica to:
Aseparate CuO as CuSiO3
Bremove calcium as CaSiO3
Cdecrease the temperature needed for roasting of Cu2S
Dremove FeO as FeSiO3
Show answer and solution
Answer: (D)
Copper pyrites contains iron. On heating in the reverberatory furnace, iron sulphide is oxidised to FeO, and the added silica acts as an acidic flux that converts this basic oxide into fusible slag: FeO+SiO2FeSiO3. The slag floats and is removed, leaving copper matte (Cu2S with some FeS). So silica is added to remove FeO as FeSiO3, option (D).
Which one of the following reactions does not occur during extraction of copper ?
A2Cu2S+3O22Cu2O+2SO2
B2FeS+3O22FeO+2SO2
CCaO+SiO2CaSiO3
DFeO+SiO2FeSiO3
Show answer and solution
Answer: (C)
In copper extraction the iron of copper pyrites is removed as slag: FeS is oxidised to FeO (B), and FeO combines with the silica flux to form FeSiO3 (D). In the converter part of Cu2S is oxidised to Cu2O (A), which then reacts with more Cu2S to give copper. Calcium silicate is the slag of the iron blast furnace, where CaO from limestone meets silica; it is not formed in copper extraction. So the answer is (C).
List IA. Reverberatory furnaceB. Electrolytic cellC. Blast furnaceD. Zone refining furnaceList III. Pig ironII. AluminiumIII. SiliconIV. Copper
AA−IV, B−II, C−I, D−III
BA−I, B−IV, C−II, D−III
CA−I, B−III, C−II, D−IV
DA−III, B−IV, C−I, D−II
Show answer and solution
Answer: (A)
Copper matte is made by smelting the sulphide ore with silica in a reverberatory furnace (A-IV). Aluminium is obtained by electrolysis of alumina in cryolite in an electrolytic cell (Hall-Heroult process) (B-II). Haematite is reduced by coke in the blast furnace, and the product is pig iron with about 4 percent carbon (C-I). Zone refining gives the ultrapure silicon used in semiconductors (D-III). So the answer is (A).
Given below are two statements. Statement I : Pig iron is obtained by heating cast iron with scrap iron. Statement II : Pig iron has a relatively lower carbon content than that of cast iron. In the light of the above statements, choose the correct answer from the options given below.
ABoth Statement I and Statement II are correct.
BBoth Statement I and Statement II are not correct.
CStatement I is correct but Statement II is not correct
DStatement I is not correct but Statement II is correct.
Show answer and solution
Answer: (B)
Pig iron comes directly from the blast furnace and has about 4% carbon. Cast iron is made by melting pig iron with scrap iron and coke, and it has a lower carbon content of about 3%. So Statement I reverses the process and Statement II reverses the carbon order. Both statements are not correct.
The compound(s) that is(are) removed as slag during the extraction of copper is : (1) CaO (2) FeO (3) Al2O3 (4) ZnO (5) NiO Choose the correct answer from the options given below
A(3),(4) only
B(2) only
C(1),(2),(5) Only
D(1),(2) only
Show answer and solution
Answer: (B)
Copper pyrites carries iron as the main impurity. On roasting the iron sulphide is oxidised to FeO, which reacts with the silica flux: FeO+SiO2FeSiO3. Iron silicate is the slag removed in copper extraction. CaO, Al2O3, ZnO and NiO are not the oxides removed as slag in this process, so only (2) is correct.
In the metallurgical extraction of copper, following reaction is used : FeO+SiO2FeSiO3 FeO and FeSiO3 respectively are.
Agangue and flux.
Bflux and slag
Cslag and flux.
DGangue and slag
Show answer and solution
Answer: (D)
In copper extraction FeO is the unwanted earthy impurity, that is the gangue. Silica is the flux that combines with it. The product FeSiO3 is the fusible slag that is removed. So FeO and FeSiO3 are gangue and slag.
The addition of silica during the extraction of copper from its sulphide ore :-
Aconverts copper sulphide into copper silicate
Bconverts iron oxide into iron silicate
Creduces copper sulphide into metallic copper
Dreduces the melting point of the reaction mixture
Show answer and solution
Answer: (B)
Copper pyrites gives FeO on roasting, which is the main impurity. Silica acts as an acidic flux and combines with this basic oxide: FeO+SiO2FeSiO3 (slag). The slag floats on the matte and is removed. So silica converts iron oxide into iron silicate.
In the leaching of alumina from bauxite, the ore expected to leach out in the process by reacting with NaOH is :
ATiO2
BFe2O3
CZnO
DSiO2
Show answer and solution
Answer: (D)
Bauxite carries SiO2, Fe2O3 and TiO2 as impurities. When it is digested with hot concentrated NaOH, the acidic silica dissolves together with alumina: SiO2+2NaOHNa2SiO3+H2O. Fe2O3 and TiO2 do not dissolve and are filtered off as red mud. ZnO is not an impurity of bauxite. The answer is SiO2.
The chemical that is added to reduce the melting point of the reaction mixture during the extraction of aluminium is:
ACryolite
BBauxite
CCalamine
DKaolite
Show answer and solution
Answer: (A)
In the Hall-Heroult process purified alumina (m.p. about 2323 K) is mixed with cryolite Na3AlF6 (and some CaF2). This lowers the melting point of the mixture to about 1140 K and raises its electrical conductivity. So cryolite is added.
Pig iron from the blast furnace is remelted with scrap iron and coke to give cast iron, which still has about 3% carbon. Cast iron is the starting material for wrought iron (impurities oxidised in a haematite lined reverberatory furnace) and for steel. Strictly, pig iron is the raw material of cast iron and not a product of it, so option (D) fits the chemistry best. The official key gives option (C), which also lists pig iron, and that answer is kept.
Among the reactions (a)−(d), the reaction(s) that does/do not occur in the blast furnace during the extraction of iron is/are: (a) CaO+SiO2CaSiO3 (b) 3Fe2O3+CO2Fe3O4+CO2 (c) FeO+SiO2FeSiO3 (d) FeOFe+21O2
Aa
Ba and d
Cc and d
Dd
Show answer and solution
Answer: (C)
In the blast furnace limestone gives CaO, which takes up silica as the slag CaSiO3, so (a) occurs. In the upper, cooler zone CO reduces Fe2O3 to Fe3O4, so (b) occurs. FeO is reduced by CO and carbon; it does not simply decompose into Fe and O2, because ΔG∘ for that change stays positive, so (d) does not occur. FeSiO3 slag is formed in copper smelting, not in the blast furnace, so (c) also does not occur. The answer is c and d.
Pig iron carries about 4% carbon and cast iron about 3%, together with other impurities. Wrought (malleable) iron is made by oxidising these impurities in a reverberatory furnace lined with haematite, which leaves less than about 0.1% carbon. It is the purest commercial form of iron, option (B).
BThe Hall-Heroult process is used for the production of aluminium and iron.
Cleaching of bauxite using concentrated NaOH solution gives sodium aluminate and sodium silicate.
Dthe blistered appearance of copper during the metallurgical process is due to the evolution of CO2.
Show answer and solution
Answer: (C)
Hot concentrated NaOH dissolves alumina as sodium aluminate, Na[Al(OH)4], and the silica impurity as sodium silicate, while Fe2O3 stays undissolved; so (C) is correct. Cast iron is made from pig iron, not the reverse. The Hall-Heroult process is used only for aluminium. Blister copper gets its blisters from escaping SO2, not CO2.
In the extraction of copper from its sulphide ore, metal is finally obtained by the oxidation of cuprous sulphide with:
ASO2
BFe2O3
CCu2O
DCO
Show answer and solution
Answer: (C)
In the Bessemer converter part of the Cu2S is roasted to Cu2O: 2Cu2S+3O22Cu2O+2SO2. The cuprous oxide then reacts with the remaining cuprous sulphide (self-reduction): 2Cu2O+Cu2S6Cu+SO2. So the sulphide is oxidised by Cu2O (C).
Extraction of copper by smelting uses silica as an additive to remove.
ACu2O
BFeS
CFeO
DCu2S
Show answer and solution
Answer: (C)
During smelting of roasted copper pyrites, iron sulphide is oxidised to FeO, which is the main impurity. Silica acts as an acidic flux and combines with the basic FeO to form a fusible slag: FeO+SiO2FeSiO3, which floats off the copper matte. Hence silica removes FeO (C).
Iron that collects as a melt at the bottom of the blast furnace contains about 3-4.3% carbon together with small amounts of Si, P, S and Mn; it is called pig iron. Cast iron is made by remelting pig iron with scrap and coke, while wrought iron and steel need further refining. Hence pig iron (D).
Heating a sulphate does not give the metal: Fe2(SO4)3 decomposes to Fe2O3 and SO3, and FeSO4 gives Fe2O3, SO2 and SO3, so (A) and (B) fail. In (C), heating FeCl3 in air does not give FeCl2 (iron stays +3). In (D), iron burns to Fe3O4, which CO reduces stepwise in the blast-furnace temperature zones, first to FeO and then to Fe. Hence (D).
Extraction of zinc from zinc blende is achieved by
Aroasting followed by self-reduction
Belectrolytic reduction
Croasting followed by reduction with carbon
Droasting followed by reduction with another metal
Show answer and solution
Answer: (C)
Zinc blende ZnS is first concentrated and roasted in air to the oxide: 2ZnS+3O22ZnO+2SO2. The oxide is then heated with coke at about 1673 K: ZnO+CZn+CO, and zinc distils off. So the process is roasting followed by reduction with carbon (C).