Electrometallurgy and hydrometallurgy JEE Main PYQ
18 Electrometallurgy and hydrometallurgy JEE Main PYQ from 2002 to 2023, newest first. Single correct option: 18. Try each one first, then open the answer and solution under it.
Not in the JEE Main syllabus. Isolation of Metals (Metallurgy) was removed from the JEE Main chemistry syllabus from the 2024 exam and is not in the 2027 syllabus. The questions here were asked up to 2023. The chapter is still in the JEE Advanced syllabus. Deleted chemistry chapters, one by one.
Electrometallurgy and hydrometallurgy questions, newest first
JEE Main 202308 Apr Shift 1
Single correct optionMarks +4, -1
Which of the following metals can be extracted through alkali leaching technique?
ASn
BPb
CAu
DCu
Show answer and solution
Answer: (A)
Tin occurs as cassiterite SnO2, an amphoteric oxide that dissolves in hot alkali: SnO2+2NaOH+2H2ONa2[Sn(OH)6]. The stannate solution is separated from the insoluble gangue and tin is then recovered. Gold is leached with cyanide, and lead and copper sulphide ores are concentrated by froth flotation, not by alkali. So the answer is Sn, option (A).
Given below are two statements: Statement I: During Electrolytic refining, the pure metal is made to act as anode and its impure metallic form is used as cathode. Statement II: During the Hall-Heroult electrolysis process, purified Al2O3 is mixed with Na3AlF6 to lower the melting point of the mixture. In the light of the above statements, choose the most appropriate answer from the options given below:
AStatement I is incorrect but Statement II is correct
BBoth Statement I and Statement II are incorrect
CStatement I is correct but Statement II is incorrect
DBoth Statement I and Statement II are correct
Show answer and solution
Answer: (A)
In electrolytic refining the impure metal is the anode, where it dissolves, and a thin strip of pure metal is the cathode, where pure metal deposits; Statement I has them reversed, so it is incorrect. In the Hall-Heroult process cryolite Na3AlF6 (with some CaF2) is mixed with alumina to lower the melting point and raise the conductivity, so Statement II is correct. The answer is (A).
The metal which is extracted by oxidation and subsequent reduction from its ore is :
AAl
BAg
CCu
DFe
Show answer and solution
Answer: (B)
Silver is extracted by the cyanide process. The ore is leached with dilute NaCN in air, and silver is oxidised from 0 to +1 as the soluble complex: 4Ag+8CN−+O2+2H2O4[Ag(CN)2]−+4OH−. Zinc then reduces it back to the metal: 2[Ag(CN)2]−+Zn[Zn(CN)4]2−+2Ag. Al, Cu and Fe are obtained by reduction of their oxides or by electrolysis, without a first oxidation of the metal. So the answer is Ag, option (B).
In isolation of which one of the following metals from their ores, the use of cyanide salt is commonly not involved?
AZinc
BSilver
CGold
DCopper
Show answer and solution
Answer: (D)
Silver and gold are leached with dilute NaCN or KCN in air, 4M+8CN−+2H2O+O24[M(CN)2]−+4OH− (M = Ag, Au), and the metal is then displaced by zinc. In zinc metallurgy a cyanide (NaCN or KCN) is used as the depressant for ZnS when a ZnS-PbS ore is concentrated by froth floatation. No cyanide salt is commonly used in the isolation of copper from its sulphide ore (froth floatation, roasting, smelting, self-reduction). So the answer is copper.
Statement I: Leaching of gold with cyanide ion in absence of air / O2 leads to cyano complex of Au (III). Statement II: Zinc is oxidized during the displacement reaction carried out for gold extraction. In the light of the above statements, choose the correct answer from the options given below.
ABoth Statement 1 and statement 2 are correct
BBoth Statement 1 and statement 2 are incorrect
CStatement 1 is correct but statement 2 is incorrect
DStatement 1 is incorrect but statement 2 is correct
Show answer and solution
Answer: (D)
Gold dissolves only when air or O2 is present, and the complex formed is [Au(CN)2]− with gold in the +1 state: 4Au+8CN−+2H2O+O24[Au(CN)2]−+4OH−. So Statement 1 is incorrect. In 2[Au(CN)2]−+Zn[Zn(CN)4]2−+2Au zinc goes from 0 to +2, so it is oxidised and Statement 2 is correct.
List-IA. Concentration of gold oreB. Leaching of aluminaC. Froth stabiliserD. Blister copperList-III. AnilineII. NaOHIII. SO2IV. NaCN Choose the correct answer from the options given below.
A(A)−(IV),(B)−(III),(C)−(II),(D)−(I)
B(A)−(IV),(B)−(II),(C)−(I),(D)−(III)
C(A)−(III),(B)−(II),(C)−(I),(D)−(IV)
D(A)−(II),(B)−(IV),(C)−(III),(D)−(I)
Show answer and solution
Answer: (B)
Gold ore is concentrated by leaching with dilute NaCN in air, so A-IV. Alumina is leached from bauxite with hot NaOH as sodium aluminate, so B-II. Aniline and cresols act as froth stabilisers, so C-I. Blister copper gets its blistered look from escaping SO2 as the copper solidifies, so D-III. The match is A-IV, B-II, C-I, D-III.
Leaching of gold with dilute aqueous solution of NaCN in presence of oxygen gives complex [A], which on reaction with zinc forms the elemental gold and another complex [B]. [A] and [B], respectively are
A[Au(CN)2]− and [Zn(CN)4]2−
B[Au(CN)4]− and [Zn(CN)2(OH)2]2−
C[Au(CN)2]− and [Zn(OH)4]2−
D[Au(CN)4]2− and [Zn(CN)6]4−
Show answer and solution
Answer: (A)
Gold dissolves in cyanide solution in air: 4Au+8CN−+2H2O+O24[Au(CN)2]−+4OH−, so A is [Au(CN)2]−. Zinc then displaces gold: 2[Au(CN)2]−+Zn[Zn(CN)4]2−+2Au, so B is [Zn(CN)4]2−.
Which of the following chemical reactions represents Hall-Heroult Process?
ACr2O3+2AlAl2O3+2Cr
B2Al2O3+3C4Al+3CO2
CFeO+COFe+CO2
D2[Au(CN)2]−(aq)+Zn(s)2Au(s)+[Zn(CN)4]2−
Show answer and solution
Answer: (B)
The Hall-Heroult process is the electrolysis of alumina dissolved in molten cryolite with graphite electrodes. Al is set free at the cathode and the oxygen formed at the anode burns the carbon anode. The overall change is 2Al2O3+3C4Al+3CO2. The other reactions are the thermite reduction, reduction of FeO in the blast furnace and the cyanide process for gold.
Given below are two statements : one is labelled as Assertion (A) and the other is labelled as Reason (R). Assertion (A) : Aluminium is extracted from bauxite by the electrolysis of molten mixture of Al2O3 with cryolite. Reason (R) : The oxidation state of Al in cryolite is +3. In the light of the above statements, choose the most appropriate answer from the options given below :
ABoth (A) and (R) are correct and (R) is the correct explanation of (A).
B(A) is true but (R) is false.
CBoth (A) and (R) are correct but (R) is not the correct explanation of (A).
D(A) is false but (R) is true.
Show answer and solution
Answer: (C)
In the Hall-Heroult process purified alumina is electrolysed in molten cryolite, so (A) is correct. Cryolite is Na3AlF6, where Al is +3, so (R) is also correct. Cryolite is added because it lowers the melting point and raises the conductivity of the melt, not because of the oxidation state of Al. So (R) does not explain (A).
In the Hall-Heroult process, aluminium is formed at the cathode. The cathode is made out of:
APlatinum
BCarbon
CCopper
DPure aluminium
Show answer and solution
Answer: (B)
The Hall-Heroult cell is a steel tank lined with carbon; this carbon lining is the cathode, at which Al3++3e−Al and molten aluminium collects. Graphite rods dipping into the melt act as the anode. Hence carbon (B).
The electrolytes usually used in the electroplating of gold and silver, respectively, are:
A[Au(NH3)2]+ and [Ag(CN)2]−
B[Au(CN)2]− and [AgCl2]−
C[Au(OH)4]− and [Ag(OH)2]−
D[Au(CN)2]− and [Ag(CN)2]−
Show answer and solution
Answer: (D)
Electroplating needs a stable complex that keeps the free metal-ion concentration low, giving a smooth, adherent deposit. Gold and silver both form very stable linear dicyano complexes, [Au(CN)2]− and [Ag(CN)2]−, which are the usual plating baths; the ammine, chloro and hydroxo complexes listed are not stable enough or not used. Hence (D).
In the Hall-Heroult cell alumina dissolved in molten cryolite is electrolysed: Al3++3e−Al at the cathode, and oxide ions are discharged at the carbon anode, which is burnt to CO2 (and CO). The overall change is 2Al2O3+3C4Al+3CO2. (A) is the thermite process, (C) is hydrometallurgical reduction of copper and (D) is carbon reduction of zinc oxide. Hence (B).
In the leaching method, bauxite ore is digested with a concentrated solution of NaOH that produces 'X'. When CO2 gas is passed through the aqueous solution of 'X', a hydrated compound 'Y' is precipitated. 'X' and 'Y' respectively are.
ANa[Al(OH)4] and Al2(CO3)3⋅xH2O
BAl(OH)3 and Al2O3⋅xH2O
CNaAlO2 and Al2(CO3)3⋅xH2O
DNa[Al(OH)4] and Al2O3⋅xH2O
Show answer and solution
Answer: (D)
Amphoteric alumina dissolves in hot concentrated NaOH under pressure (473-523 K, 35-36 bar) as sodium aluminate: Al2O3+2NaOH+3H2O2Na[Al(OH)4], so X is Na[Al(OH)4]. Passing CO2 neutralises the solution and hydrated alumina precipitates: 2Na[Al(OH)4]+CO2Al2O3⋅xH2O+2NaHCO3, so Y is Al2O3⋅xH2O. Hence (D).
In the context of the Hall-Heroult process for the extraction of Al, which of the following statements is false?
ANa3AlF6 serves as the electrolyte.
BCO and CO2 are produced in this process.
CAl2O3 is mixed with CaF2 which lowers the melting point of the mixture and brings conductivity.
DAl3+ is reduced at the cathode to form Al.
Show answer and solution
Answer: (A)
In the Hall-Heroult cell the substance electrolysed is alumina dissolved in the melt; cryolite Na3AlF6 and CaF2 only act as solvent/flux, lowering the melting point and raising conductivity, so (C) is true and (A) is false. At the cathode Al3++3e−Al (true), and oxygen released at the graphite anode burns it to CO and CO2 (true). Hence the false statement is (A).
In the electrolysis of alumina to obtain aluminium metal, cryolite is added mainly to
Alower the melting point of alumina
Bdissolve alumina in molten cryolite
Cremove the impurities of alumina
Dincrease the electrical conductivity
Show answer and solution
Answer: (A)
Alumina melts at about 2323 K and its melt is a poor conductor. Mixing it with cryolite Na3AlF6 (and some fluorspar CaF2) brings the operating temperature of the bath down to about 1140-1240 K, which saves energy, and also improves conductivity. The key takes the lowering of melting point as the main purpose, answer (A).
In the cyanide process the silver ore is leached with dilute aqueous NaCN in the presence of air, which takes silver into solution as the soluble complex [Ag(CN)2]−. Zinc is then added, and being more electropositive it displaces silver: 2[Ag(CN)2]−+Zn[Zn(CN)4]2−+2Ag. Barium, aluminium and boron are not extracted this way, so the answer is silver (D).
Leaching with cyanide is used for the noble metals silver and gold. Argentite reacts with sodium cyanide to give soluble sodium dicyanoargentate(I): Ag2S+4NaCN2Na[Ag(CN)2]+Na2S (air oxidises the sulphide and drives the reaction). Scrap zinc then precipitates the metal: 2Na[Ag(CN)2]+ZnNa2[Zn(CN)4]+2Ag. Hence the metal is Ag (B).
Pure alumina melts above 2300 K and its melt conducts poorly, so it is not electrolysed alone. In the Hall-Heroult process purified alumina is dissolved in molten cryolite Na3AlF6 (with some CaF2), which lowers the melting temperature to about 1240 K and raises conductivity. Aluminium is discharged at the cathode, so the answer is (C).