MolSynapse
question bank
All chapters
NEET
JEE
Practice
MolSynapse
/
Question bank
/
Polymers
/
Rubber and vulcanisation
JEE Main level
Single correct option
Difficulty 2 of 3
pl204
Complete catalytic hydrogenation of natural rubber saturates every
C
=
C
. The molar mass of the saturated repeat unit (C 12, H 1) is
A
66
B
68
C
70
D
72
Answer: C
The unsaturated repeat unit
C
X
5
H
X
8
has one
C
=
C
and adds one
H
X
2
to become
C
X
5
H
X
10
. Its mass is
5
×
12
+
10
=
70
.
Practice Polymers
More on Rubber and vulcanisation
Previous question
Next question
More questions on Rubber and vulcanisation
The mass percentage of chlorine in neoprene (repeat unit -[CH2-C(Cl)=CH-CH2]-, C 12, H 1, Cl 35.5) is closest to
JEE Main level
The monomer unit of natural rubber is
NEET level
Which of the following statements about natural rubber and gutta-percha is/are correct? (One or more options may be correct.)
JEE Advanced level
A 100 g sample of natural rubber (repeat unit C5H8, 68 g/mol) is vulcanised with 3.2 g of sulfur (S = 32). Assume all the sulfur is present ...
JEE Main level
Buna-S contains styrene and buta-1,3-diene units in the mole ratio 1 : 3 (end groups ignored; C 12, H 1). The mass percentage of carbon in t...
JEE Advanced level
During vulcanisation, sulfur cross-links form chiefly at
JEE Main level